posted on 2014-05-12, 03:45authored byYaotao Wang, Zhiyong Jiang, Lianlian Fu, Ying Lu, Yongfeng Men
The 2D-WAXD patterns taken at different strains as indicated on the graph for PB-1 samples crystallized at 50°C stretched at 30 (top) and 100°C (middle), and the ones crystallized at 90°C stretched at 100°C (bottom). Stretching direction is horizontal. Arrows indicate the azimuthal angle of intensity distribution.