Figure_11.tif (2.34 MB)
3D AFM images of the Ti-6Al-4V alloy with an acid-etched surface.
figure
posted on 2014-03-26, 03:10 authored by Leonardo P. Faverani, Wirley G. Assunção, Paulo Sérgio P. de Carvalho, Judy Chia-Chun Yuan, Cortino Sukotjo, Mathew T. Mathew, Valentim A. BaraoSurfaces were characterized before (baseline) and after corrosion in SBF (control) with different concentrations of dextrose (DEX) and lipopolysaccharide (LPS), alone or in association (DEXLPS).
History
Usage metrics
Categories
Keywords
BiochemistryglycobiologypolysaccharidesbiotechnologybiomaterialsgeneticsHuman geneticsClinical geneticsMitochondrial diseasesDiabetes mellitus and deafnessOral medicinedentistrychemistryChemical reactionscorrosionElectrochemistryMaterials ScienceMaterials by structureIntermetallicsDental amalgamsComposite materialsMaterials physicsmicrostructureMaterial propertiesMaterials characterizationafmimagesti-6al-4valloyacid-etched